Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3U42G6 - (PA66+PA6)-GF30 FR(40) - BASF

Material Data Center offers the following functions for Ultramid® A3U42G6:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Without halogenes flame retarded glass fiber reinforced injection moulding grade; light colorable; outstanding mechanical and electrical properties.
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 20 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carico 5 / * kg -
Ritiro di stampaggio, parallelo 0.3 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 10800 / 7400 MPa ISO 527
Carico unitario a rottura 130 / 90 MPa ISO 527
Deformazione a rottura 3 / 4.5 % ISO 527
Modulo a flessione, 23°C 11000 / 7500 MPa ISO 178
Resistenza all'urto Charpy, +23°C 60 / 65 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 55 / 60 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 8 / 11 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 7 / 7 kJ/m² ISO 179/1eA
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 260 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 230 / * °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 250 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 22 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 79 / * E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 / * class IEC 60695-11-10
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco a spessore h V-0 / * class IEC 60695-11-10
Spessore provato 0.4 / * mm -
Yellow Card disponibile sì / * - -
Reazione al fuoco 5V a spess. h 5VA / * class IEC 60695-11-20
Spessore provato 1.6 / * mm -
Yellow Card disponibile sì / * - -
Indice di ossigeno 37 / * % ISO 4589-1/-2
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 3.9 / 4.1 - IEC 62631-2-1
Fattore di dissipazione, 1MHz 150 / 290 E-4 IEC 62631-2-1
Resistività volumica 1E11 / 1E9 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E13 Ohm IEC 62631-3-2
Rigidità dielettrica 38 / 30 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali - / 600 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 5 / * % Sim. alla ISO 62
Assorbimento d'umidità 1.7 / * % Sim. alla ISO 62
Massa volumica 1440 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 °C -
Pre-essiccamento - Tempo 4 h -
Umidità del Processo ≤0.15 % -
Temperatura di fusione 280 - 300 °C -
Temperatura dello stampo 80 - 90 °C -
Funzioni
Sforzi-deformazione , Ultramid® A3U42G6 (Secco), (PA66+PA6)-GF30 FR(40), BASF
Sforzi-deformazione , Ultramid® A3U42G6 (cond.), (PA66+PA6)-GF30 FR(40), BASF
Modulo secante-deformazione , Ultramid® A3U42G6 (Secco), (PA66+PA6)-GF30 FR(40), BASF
Modulo secante-deformazione , Ultramid® A3U42G6 (cond.), (PA66+PA6)-GF30 FR(40), BASF
Modulo a taglio-temperatura , Ultramid® A3U42G6 (Secco), (PA66+PA6)-GF30 FR(40), BASF
Modulo a taglio-temperatura , Ultramid® A3U42G6 (cond.), (PA66+PA6)-GF30 FR(40), BASF
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Pellet
Additivi
Agente di distacco
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni
Disponibilità geografica
Nord America, Europa
Altre informazioni
Stampaggio ad Iniezione
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.